Clay component brick is usually made of high quality clay or even purple clay, then fired at high temperature. It use natural clay as the main component, quartz and feldspar as aggregates, then formed civil building wall brick after sintering.
The nature of clay component brick belongs to low temperature brick, burning temperature is about 800℃, water absorption rate is higher, the general water absorption rate is 8%- 10%.
Characteristics:
It can freeze and thaw 50 times at -45℃ without cracks.
It can refract more than 90% of the light, which can protect human vision and reduce light pollution.
It can refract all or part of the sound wave, reduce the outdoor noise and eliminate the indoor echo.
Breathable and permeable;Alkali corrosion resistance.